Monel 500 Bolts for Hydrofluosilicic Acid

Q:  What is the best alloy to bolt to use in a flange on the outside Hydrofluosilicic acid storage tank?

A: Probably the best materials for Hydrofluosilicic acid bolting would be a Monel K500 bolt. This material will give you the strength and good corrosion resistance to the this very aggressive acid. Monel K500 bolts also offer high strength approximately 3 times the yield strength (110ksi vs 45ksi) and double the tensile strength (160ksi vs 83ksi) when compared grade 400.

This entry was posted in Application, Corrosion Resistance, FAQs, Material, Specialty Metal Fasteners, Technical Questions and tagged , , , , , , , , , , , . Bookmark the permalink.

Leave a Reply

Your email address will not be published. Required fields are marked *

Questions?

Our material experts are ready to help guide you through your specific application.