Q: What heat treatment would you recommend for 17-4PH exposed to salt water? Can I use H900? A: H900 is susceptible to chloride stress corrosion cracking. 17-4 with salt exposure should be H1025 or higher. And, best practice it to use the highest heat treat temp that works for an … Continue reading →
Posted in Application, Corrosion Resistance, FAQs, High Strength, Specialty Metal Fasteners, Technical Questions | Tagged 17-4 for saltwater resistnace, 17-4 in saltwater, 17-4 saltwater corrosion resistance, 17-4 stress corrosion cracking, 17-4PH for saltwater resistance, 17-4PH in saltwater, 17-4PH saltwater resistance, 17-4PH stress corrosion cracking, 174PH in saltwater, H1025 for saltwater, H900 for saltwater | Leave a comment