Posted on May 24, 2017 by dean
Q: I’m running a steam surface condenser which is installed on a steam turbine in a thermal power station. I’m using sea water that could be contaminated with chemical pollutants cooling water side of the condenser. Any ideas on a good fastener for the tubes and water boxes? A: Duplex 2205 … Continue reading →
Posted in Application, Corrosion Resistance, FAQs, High Temperature Resistance, Specialty Metal Fasteners, Technical Questions | Tagged AL6XN, Alloy 2205, chloride corrosion, Corrosion, Crevice Corrosion, Duplex, Duplex 2205, High Temperature, pitting corrosion, salt water corrosion, Steam condenser, steam surface condenser, Stress Corrosion Cracking | Leave a comment
Posted on April 27, 2017 by dean
Q: We have a pulp & paper digester that is used to cook wood chips in an alkaline solution. The fasteners will be exposed to high temperatures and abrasive conditions. Any suggestions? A: Without knowing the specifics of your process, I can make two general material suggestions. Duplex 2205 fasteners are … Continue reading →
Posted in Application, Corrosion Resistance, FAQs, High Temperature Resistance, Material, Specialty Metal Fasteners, Technical Questions | Tagged alkaline, Alloy 2205, Alloy C276, Chlorides, Crevice Corrosion, Digester, Duplex 2205, Duplex Steel, Hastelloy, Hastelloy C276, pitting corrosion, Pulp & Paper, Pulp & paper digester, Stress Corrosion Cracking | Leave a comment