Tag Archives: Galvanic corrosion resistance in salt water
Posted on February 23, 2023 by Kathleen
Q: I want to use Duplex bolts to bolt down a Monel plate. Will these materials be compatible? A: When you mean compatible, I’m assuming you are referring to galvanic corrosion. Galvanic corrosion is when two dissimilar metals create an electrochemical reaction and corrosion occurs. Duplex and Monel can experience … Continue reading →
Posted in Application, Corrosion Resistance, FAQs, Material, Specialty Metal Fasteners, Technical Questions | Tagged Bolt Galvanic Corrosion, Can monel and duplex experience galvanic corrosion, Does water cause galvanic corrosion, Fastener Galvanic Corrosion, Galvanic corrosion resistance in salt water, Galvanic Corrosion to Bolts, Galvanic Corrosion to Fasteners, Screw Galvanic Corrosion, What causes bolts galvanic corrosion, What causes galvanic corrosion, What causes galvanic corrosion to bolts, What causes galvanic corrosion to screws, When does galvanic corosion occur, Will galvanic corrosion happen if materials are dry, Will galvanic corrosion happen if materials are wet, Will galvanic corrosion occur if materials are dry, Will galvanic corrosion occur if materials are wet | Leave a comment
Posted on April 9, 2018 by dean
Q: I need a salt water corrosion resistant screw that will work well to fasten an aluminum housing for deep sea equipment. I am concerned about galvanic corrosion. What material should I consider? A: Since you are using fasteners in an ocean environment and in contact with aluminum you have … Continue reading →
Posted in Application, Corrosion Resistance, FAQs, Specialty Metal Fasteners, Technical Questions | Tagged Galvanic corrosion of aluminum and titanium, Galvanic corrosion of titanium and aluminum, Galvanic corrosion resistance in salt water, galvanic corrosion resistant bolt, galvanic corrosion resistant bolt salt water, galvanic corrosion resistant fastener, galvanic corrosion resistant fastener salt water, galvanic corrosion resistant screw, galvanic corrosion resistant screw salt water, salt water galvanic corrosion resistance, Titanium and Aluminum Galvanic Corrosion, Titanium bolt galvanic corrosion, titanium fastener galvanic corrosion resistance, Titanium Galvanic corrosion, titanium galvanic corrosion resistance in salt water, titanium galvanic corrosion resistance salt water, titanium screws galvanic corrosion | Leave a comment