Q: Will Nickel 200 bolts be a good choice for hydrofluoric acid? A: For aqueous HF, Nickel 200 fasteners offer limited protection. If application requires a metal then you may want to consider Monel 400. Monel 400 bolts are the most resistant option for hydrofluoric acid in all concentrations up … Continue reading →
Posted in Application, Corrosion Resistance, Engineered Polymer Fasteners, FAQs, Material, Specialty Metal Fasteners, Technical Questions | Tagged Monel 400 bolts for HF corrosion, Monel 400 bolts for hydrofluoric acid corrosion, Monel 400 fasteners for HF corrosion, Monel 400 fasteners for hydrofluoric acid corrosion, Monel 400 for hydrofluoric acid corrosion, Monel 400 screws for hydrofluoric acid corrosion, PTFE bolts for HF corrosion, PTFE bolts for hydrofluoric acid corrosion, PTFE fasteners for HF corrosion, PTFE fasteners for hydrofluoric acid corrosion, PTFE screws for HF corrosion, PTFE screws for hydrofluoric acid corrosion, PVDF bolts for HF corrosion, pvdf bolts for hydrofluoric acid corrosion, PVDF fasteners for HF corrosion, pvdf fasteners for hydrofluoric acid corrosion, PVDF screws for HF corrosion, pvdf screws for hydrofluoric acid corrosion | Leave a comment